Knowledge Base › Design Pitfalls › Casting Design

Design Pitfalls · Casting Design (Quick-Reference Handbook)

Abrupt Wall-Thickness Change in Castings

Pitfall: wall-thickness ratio between adjacent walls >3:1

Consequence: shrinkage cavities / hot spots / cracks at the thick-to-thin transition

Correct practice: wall-thickness ratio ≤2:1 / provide a transition fillet

No Draft Angle on Castings

Pitfall: vertical walls perpendicular to the parting plane have no draft angle

Consequence: cannot be ejected / the mold is scored

Correct practice: draft angle 1~3° for outer walls / 2~5° for inner walls

Sharp Corners Without Fillets in Castings

Pitfall: the junctions of inner / outer walls are sharp corners (R=0)

Consequence: stress concentration → cracking / sand holes

Correct practice: inner R≥0.2× wall thickness / outer R≥0.5× wall thickness

Casting Structural Design Pitfalls

① Pitfall: uneven wall thickness

Correct practice: keep the wall thickness as uniform as possible, and add fillets where the thickness changes

② Pitfall: sharp corners

Correct practice: design casting fillets at all corners

③ Pitfall: walls crossing in a cross shape

Correct practice: change to a T shape or an offset (staggered) intersection

④ Pitfall: a large flat face placed horizontally

Correct practice: add a slope to aid venting and mold filling

⑤ Pitfall: inner walls too thick

Correct practice: make the inner-wall thickness 0.8× the outer wall

⑥ Pitfall: the casting has no draft angle

Correct practice: 1°~3° for outer walls, 2°~5° for inner walls

⑦ Pitfall: a hot spot forms where stiffening ribs intersect

Correct practice: stagger the rib intersections

⑧ Pitfall: cast holes too small

Correct practice: minimum cast hole diameter ≥30mm for sand casting

Casting Draft Not Marked

[Casting Draft Callout] Casting draft angle 2~5° for inner walls / 1~3° for outer walls / it should be marked on the drawing / no callout → the mold is made without draft → difficult ejection

Casting Burrs Not Cleaned

[Casting Burrs Not Cleaned After Cooling] After sand removal, castings should have flash and burrs ground off / not cleaned → affects positioning during assembly / cuts the operator

Casting Wall Thickness Too Thick

Design pitfall: when the casting wall thickness >25mm, internal shrinkage porosity readily forms / make it hollow / add ribs / reduce the wall thickness / ensure soundness

Other quick references in this series:Welding PitfallsCasting PitfallsShaft System PitfallsSheet Metal PitfallsAssembly PitfallsHydraulic PitfallsPneumatic PitfallsShaft System DesignHousing DesignWelded StructuresSheet Metal StructuresSpring DesignBolted JointsBearing Arrangement

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »