Knowledge Base › Design Pitfalls › Sheet-Metal Design

Design Pitfalls · Sheet-Metal Design (Quick-Reference Handbook)

Burr Direction of Sheet-Metal Blanking Not Marked

Pitfall: the sheet-metal part drawing does not mark the burr direction (blanking direction)

Consequence: conflicting burr directions during assembly → poor seating / scratches

Correct practice: mark the burr orientation (or specify deburring)

Bend Too Close to a Hole in a Sheet-Metal Part

Pitfall: the bend line sits right next to an existing hole (distance <3t)

Consequence: the hole is stretched out of shape (elliptical)

Correct practice: hole distance from the bend line ≥3t / bend first, then punch

Sheet-Metal Structural Design Pitfalls

① Pitfall: bend radius too small

Correct practice: R≥t (perpendicular to the fiber direction), R≥2t (parallel to the fiber direction)

② Pitfall: bend edge too short

Correct practice: bend edge height H≥3t

③ Pitfall: hole too close to the bend line

Correct practice: hole edge distance from the bend line ≥3t

④ Pitfall: sharp right-angle corners on a square hole

Correct practice: R≥0.3t at the four corners of a square hole

⑤ Pitfall: the minimum blanking hole diameter is smaller than the sheet thickness

Correct practice: minimum hole diameter d≥t (steel sheet)

⑥ Pitfall: no process notch at the bend corner

Correct practice: provide a process notch with width ≥t and depth ≥2t

⑦ Pitfall: excessive draw depth formed in a single operation

Correct practice: draw in multiple steps, with a draw ratio ≥0.5 each time

⑧ Pitfall: flange (formed edge) height too large

Correct practice: flange height ≤3t (single-pass flanging)

Sheet-Metal Bend Inner Radius Too Small

When the bend inner radius R< sheet thickness t, the outer surface cracks / low-carbon steel R≥t / stainless steel R≥2t / aluminum R≥1.5t / if unavoidable, cut a process relief groove

Insufficient Bend Edge Distance in Sheet Metal

Distance from the bend line to the edge <3t → the edge tears under stretching / should be ≥3t (preferably ≥5t) / ≥2.5t for L-shaped parts / if unachievable, add extra material and trim afterwards

Blanked Parts Spaced Too Closely in Sheet Metal

Spacing between adjacent blanked parts <2t → short die life / large burrs / should be ≥2t (≥3t recommended) / edge distance ≥t

No Process Notch in Sheet Metal

A process notch (crack-stop slot) with R≥1mm should be cut where sheet-metal bends intersect / without it → the intersection tears / notch width ≥2t

Stiffening Rib Too Shallow in Sheet Metal

Sheet-metal stiffening rib depth <3t → almost no stiffening effect / should be ≥5t (ideally ≥10t) / rib width ≥3t / rib spacing ≥5t

Insufficient Flange Height in Sheet Metal

Flange height <3t → the flange cracks / should be ≥4t (5t recommended) / pre-punch the hole before flanging / ensure the hole diameter is accurate after flanging

Deburring Direction of the Sheet-Metal Part Not Marked

The blanking burr direction should be marked on the drawing / burr orientation should be consistent / or specify deburring (chamfer ≤0.2×45°)

Blanked Hole Too Close to the Bend in Sheet Metal

Hole center distance from the bend line <3t → the hole deforms / should be ≥3t (bending first and punching afterwards is better) / or cut a slotted hole to compensate

Lack of Positioning for a Weld Nut on Sheet Metal

A weld nut on sheet metal without positioning (a punched locating hole / raised boss) → the nut is offset → the bolt cannot be installed / provide positioning

Minimum Edge Distance for a Threaded Hole in Sheet Metal

For a flanged-and-tapped threaded hole in sheet metal, hole center distance from the sheet edge <2d → insufficient strength / should be ≥2d+1mm / or thicken the edge

Corner Radius Too Small on a Sheet-Metal Drawn Part

For drawn parts, bottom R≥3t / flange R≥2t / too small → the bottom tears during drawing / increase the corner radius or draw in multiple steps

Excessive Draw Depth in Sheet Metal

Single-pass draw depth ≤0.4~0.6× the diameter / too deep → the part tears / draw in multiple steps / anneal in between to soften

Improper Blanking Clearance in Sheet Metal

Blanking die clearance = sheet thickness × 5~10% / clearance too small → large burrs / too large → rough sheared surface / select accurately per the standard

Sheet-Metal Bend Direction Parallel to the Rolling Direction

Keep the bend line perpendicular to the sheet rolling direction as far as possible / bending parallel to the rolling direction → the outer surface tends to crack / increase R if unavoidable

No Stress-Relief Heat Treatment for the Sheet-Metal Part

After multiple bends / draws, sheet metal should be stress-relief annealed / skipping it → high internal stress → distortion / unstable accuracy

Unclear Datum on the Sheet-Metal Part

Sheet-metal part dimensions should use a single unified datum (take one edge or hole as the datum) / multiple datums → accumulated error → difficult assembly

Wrong Die Used for Bending Stainless-Steel Sheet Metal

Bending stainless steel requires a dedicated die (with greater rigidity) / an ordinary carbon-steel die → the die wears quickly → inaccurate bend R

Insufficient Hole-Flange Height for Tapping in Sheet Metal

For hole flanging and tapping (M3~M6), the flange height should be ≥3× the thread pitch / insufficient → too few threads → thread stripping / calculate the pre-punched hole diameter before flanging

No Compensation for Springback in Sheet-Metal Bending

Sheet-metal bending exhibits springback (about 1~3°) / compensate with an angle in the die / without compensation → inaccurate bend angle / trial-bend and then adjust the die

Stainless-Steel Sheet Metal Bends at a Larger Angle Than Ordinary Steel

Stainless steel (304) has 2~3° more springback than ordinary steel / over-bend or increase the die compensation angle / without compensation → the angle is out of tolerance

Sheet-Metal Bend R Too Small

Design pitfall: minimum bend radius of a bent part ≥0.5t (carbon steel) ≥1t (stainless steel) ≥1.5t (aluminum) / too small → the outer surface cracks

Sheet-Metal Part Bend Without an Inner/Outer R Callout

The sheet-metal bend R should be marked (inner R or outer R) / no callout → no basis for die manufacture → inaccurate bend angle / dimensional deviation after bending

No Deburring Requirement for Blanked Sheet-Metal Parts

Blanked parts have burrs at the edges / the drawing should specify deburring (chamfer ≤0.2×45°) / no deburring → scratches during assembly / cut hands

Mismatch Between Hole-Flange Diameter and Flange Height in Sheet Metal

Flange height H≈(D-d)/2+0.5t / too high → the flange edge thins → cracks / too low → too few threads

No Shrinkage Allowance Left in the Length Direction of the Sheet-Metal Part

Sheet-metal parts shrink in length after bending (about 0.5~1mm/m) / account for this during design / bending after finishing gives higher accuracy

Ratio of Sheared (Bright) Band to Fracture Band on a Blanked Part

With proper blanking clearance, the sheared band ≈1/3 of the section / clearance too small → a large sheared band / too large → large burrs / set clearance from empirical data

No Springback Compensation After Bending Stainless-Steel Sheet Metal

Stainless-steel bending springback angle ≈3~5° / needs die compensation / without compensation → the bend angle is too large / measure and correct after bending

Sheet-Metal Part Callout Omits Thickness Tolerance

Sheet-metal thickness has a tolerance (hot-rolled sheet ±0.5mm / cold-rolled sheet ±0.2mm) / no callout → fasteners do not tighten properly during assembly

No Dwell Angle Specified for Sheet-Metal Laser Cutting

When laser-cutting thick sheet metal (>6mm) / set a dwell (corner delay time) at the corners to avoid corner overburn

Stainless-Steel Surface Left Unprotected

Stainless-steel sheet metal should have a protective film applied / without protection → scratches → the finished product fails the appearance requirement

Blank Size Not Called Out on Drawn Parts

Drawn parts should call out the blank size / no callout → the blank size cannot be calculated

Other quick references in this series:Welding PitfallsCasting PitfallsShaft System PitfallsSheet Metal PitfallsAssembly PitfallsHydraulic PitfallsPneumatic PitfallsShaft System DesignHousing DesignWelded StructuresSheet Metal StructuresSpring DesignBolted JointsBearing Arrangement

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »