Pitfall: tapped hole depth in a steel part <1.5 times the bolt diameter
Consequence: insufficient joint strength / thread stripping
Correct practice: thread engagement ≥1.5d in steel
Pitfall: tapped hole depth in a cast iron part <2 times the bolt diameter
Consequence: insufficient threaded joint strength
Correct practice: thread engagement ≥2d in cast iron
Pitfall: tapped hole depth in an aluminum alloy part <2.5 times the bolt diameter
Consequence: aluminum alloy has low strength → thread pull-out
Correct practice: thread engagement ≥2.5d in aluminum (a wire thread insert is even better)
Pitfall: locking a critical tension bolt with a spring washer only
Consequence: it still loosens under prolonged vibration
Correct practice: use a nylon-insert locknut / anaerobic adhesive / double nut + cotter pin
Pitfall: bolt spacing <1.5d (a wrench cannot reach it)
Consequence: the bolt cannot be tightened/loosened
Correct practice: wrench clearance ≥d+6mm (box-end wrench) or ≥d+10mm (open-end wrench)
Pitfall: bolts unevenly distributed on the same joint face (dense on one side, sparse on the other)
Consequence: uneven clamping of the joint face → leakage / deformation
Correct practice: distribute bolts symmetrically and evenly / spacing ≤10d
Pitfall: the bearing surface under the bolt head/nut is sloped (the casting was not milled flat)
Consequence: the bolt carries an eccentric load → bending → fracture
Correct practice: provide a boss (milled flat) at the bolt location or use a tapered washer
Pitfall: no vent hole at the bottom of a blind thread / depth >3d
Consequence: trapped compressed air during assembly → the bolt cannot be tightened fully
Correct practice: drill a vent hole (φ2~3mm) at the bottom of the blind hole or increase the pilot hole depth
Pitfall: countersink depth for a countersunk screw >50% of the plate thickness
Consequence: the plate is weakened too much → insufficient strength
Correct practice: countersink depth ≤1/3 of the plate thickness (load-bearing part) or ≤1/2 (non-load-bearing)
Pitfall: low stiffness / thin walls / no ribs on the joined parts (they deform when the bolts are tightened)
Consequence: poor joint stiffness → loss of preload / leakage
Correct practice: add ribs / increase thickness / enlarge the joint face / add washers to spread the clamping force
Bolt/nut wrench sizes must match (GB/T 4388) / M6 uses a 10mm wrench / M8 13mm / M10 16mm / M12 18mm / M14 21mm / M16 24mm / M20 30mm / M24 36mm / M30 46mm
The bolt head/nut bearing surface diameter should be ≥1.5 times the thread diameter / if smaller it sinks into the joined part surface / or add an enlarged washer
Thread engagement ≥2.5d in aluminum / if insufficient use a wire thread insert / or switch to a through stud / or thicken the aluminum part
For a blind thread deeper than >3d, drill a vent hole (φ2mm) / or extend the pilot hole to 5 times the thread pitch / to prevent trapped compressed air from stopping the bolt short of full engagement
A tapped hole closer than <2d to the plate edge gives insufficient strength / should be ≥2d (3d recommended) / or flange the edge / or add a rivet nut
Countersink diameter ≤50% of the plate thickness / ≤1/3 of plate thickness for load-bearing parts / if unavoidable, switch to a hex-head or socket-head bolt
For critical tension-bolt joints, calculate the preload at 70~80% of the material yield strength / tighten with a torque wrench / ensure the joint face is tightly closed
A bolt in shear (carrying lateral load) should be a fitted (reamed-hole) bolt (H7/m6) / or use a fitted pin to transmit the shear / ordinary bolts are only for tension
A high-strength bolt hole should be 1~2mm larger than the bolt diameter (standard hole) / or use an interference fit to transmit shear / an oversized hole reduces joint strength
Bolt hole groups should be match-drilled / match-reamed to ensure consistency / never lay out and drill them separately (large cumulative error)
Arrange a bolt group symmetrically so the load is shared evenly / avoid eccentric loading / typical bolt spacing ≤10d and at least ≥3d
Machine a boss (1~3mm high) on the bolt mounting face / or mill a spot-face / keep the bolt head bearing surface flat / do not mount on a slope
Spring washers suit only general vibration conditions / for high vibration, shock, or critical joints use a nylon-insert locknut / anaerobic adhesive / spring washer + locknut
Choose the locking method by vibration level:
Low vibration → spring washer
Medium vibration → nylon-insert locknut + flat washer
High vibration → double nut + cotter pin
Extreme → anaerobic adhesive on the threads
Stud engagement in steel ≥1.5d / cast iron ≥2d / aluminum ≥2.5d / if insufficient the joint strength is inadequate / thread pull-out
Leave ≥2mm clearance between the stud threaded end and the bottom of the tapped hole / to avoid the stud bottoming out and damaging the thread when tightened
Dowel pin holes should be match-drilled / match-reamed in both joined parts to ensure locating accuracy / never machine them separately / keep the pin holes not too far from the assembly datum
The dowel pin diameter should not be too large (choose a fit that meets the shear stress) / too large → a bigger hole → weakens the joined part / especially when the pin hole is near an edge
Select the cotter pin diameter per the bolt hole diameter (GB/T 91) / after insertion splay the ends at least 60° / too small a diameter → it shears
The lock washer (internal/external tooth, double-folded, conical) must match the bolt head/nut size / too large → it sinks in / too small → the locking fails
An anchor bolt needs to protrude >2~3 threads beyond the nut / too long → easy to bump / wasteful / if ≥10mm provide a protective cap
High-strength bolts (grade 8.8/10.9) must be tightened to the standard torque with a torque wrench / too loose → the joint loosens / too tight → the bolt breaks
Tighten a bolt group diagonally and alternately (cross pattern) / ignoring the sequence → the joint face warps / leaks / loses preload
Tighten flange bolts in 2~3 passes with increasing torque / tightening straight to final torque → the flange warps → leakage
For a self-tapping screw (p=1.6mm) the pilot hole is 1.1~1.3mm / too small → it will not go in / too large → thread stripping / confirm by test
A set screw should bear on a 90° cone or flat spot on the shaft / bearing directly on the shaft surface → it dents the shaft / locking force is insufficient
A spring washer pressed onto a copper/aluminum part → it sinks in → damages the surface → use a flat washer + threadlocker instead
Pipe thread (G/R) joints should be wrapped with PTFE tape (clockwise) / without it → thread gaps → seepage
Too much PTFE tape → the excess enters the pipe → clogs valves/nozzles / 2~3 turns is enough
A tapered pipe thread (R/NPT) driven in too deep → excessive stress → the thread cracks / drive it in until 1~2 threads remain exposed
A flat washer generally has no designated face / but a chamfered washer (GB/T 97.2) goes with the chamfer toward the nut / a spring washer goes with its gap facing the tightening direction
When a bolt is mounted on a slope/cone (such as an I-beam flange) / add a tapered washer (GB/T 852) / without it → the bolt bends → breaks
A cotter pin is a single-use part / always replace it after removal / reusing it → it breaks → the nut comes loose
A retaining ring (shaft/external or bore/internal) loses spring force after removal / replace it / if not → the ring pops out → danger
Turning a thread at the end of a slender rod (slenderness ratio >20) → stress concentration where the thread meets the plain shank → fracture / add a relief groove or roll the thread
Identical bolts/nuts/washers in the same assembly should follow one standard / mixing standards → poor fit
Tighten a bolt group diagonally in 2~3 passes / tightening each bolt once → uneven preload → warping / leakage / the cross pattern is recommended
Spot-face depth on the same joint face should be uniform (tolerance ±0.1mm) / differing depths → uneven bolt preload → the joint face warps
Chamfer the tapped hole mouth C0.5~1mm / without it → the first thread is damaged / the bolt is hard to start / burrs form
Aluminum tapped holes (where parts are removed often) should have a wire thread insert / without it → repeated assembly → thread stripping / scrapping
Self-drilling screw penetration = plate thickness +1~2mm / too deep → drills through / too shallow → weak joint / use a depth-limited bit
Bolt locking by vibration level: low → spring washer / medium → nylon-insert locknut + flat washer / high → double nut + cotter pin / extreme → anaerobic adhesive on the threads
A taper pin (1:50) hole should be match-drilled and match-reamed / without it → taper mismatch → poor locating accuracy / the pin does not seat tightly
A flat washer should sit between the bolt head/nut bearing surface and the joined part / without it → the joined part surface is crushed during tightening / preload is lost
Tapping into plate <2mm thick → too few threads → insufficient joint strength / add a rivet nut / clinch nut / weld nut
The friction face of a high-strength bolted (friction-type) joint should be blast-cleaned / coated + slip-resistant / without treatment → insufficient friction coefficient → slip
Design pitfall: threaded pilot hole too large (>0.2mm over the standard value) → the thread is too shallow → thread stripping / select the pilot drill per the standard
The bolt hole center should be ≥1.5d from the plate edge (≥2d recommended) / too small → the edge tears out / especially important for thin plate
A bolt longer than >50mm under tension tends to load eccentrically → bending → thread pull-out / increase the diameter or use a higher strength grade
A shear bolt (fitted/reamed-hole type) matches the hole H7/m6 / an ordinary bolt → clearance → lateral vibration → the joint loosens
Use high-strength bolts as complete assemblies (bolt + nut + washer from the same maker/lot) / mismatched → inconsistent torque coefficient → inaccurate preload
Over-torquing a U-bolt deforms its legs → the clamping force actually drops / tighten to the standard torque
The friction face of a high-strength bolted (friction-type) joint should be blast-cleaned (slip coefficient ≥0.45) / without treatment → insufficient friction coefficient → slip
Preload F=0.7×σs×As / torque T=0.2×F×d / without calculating → torque too high → the bolt breaks / too low → the joint loosens
A tension bolt (carrying axial load) uses an ordinary clearance-fit bolt / a fitted reamed-hole bolt → over-constraint → the bolt is hard to install
When a bolt is mounted on the sloped flange of an I-beam/channel / use a tapered washer (GB/T 852) / without it → the bolt bends → breaks
A set screw should bear on a 90° cone on the shaft (HRC≥50) / bearing directly on the shaft surface → indentation → stress concentration → the shaft breaks
Bolts on a perforated/grating plate need a relief washer under the plate / without it → the surface under the bolt head is uneven → insufficient preload → loosening
Vibrating service needs a nylon-insert locknut / all-metal locknut / an ordinary nut + spring washer → poor locking → loosening
The drawing should specify the locking requirement / without it → assembly follows convention → the joint loosens under vibration
The assembly drawing should annotate bolt thread engagement / without it → insufficient joint strength or the part is pushed through
Bolt hole center <1.5d from the edge → insufficient strength and tear-out / should be ≥2d
Other quick references in this series:Welding PitfallsCasting PitfallsShaft System PitfallsSheet Metal PitfallsAssembly PitfallsHydraulic PitfallsPneumatic PitfallsShaft System DesignHousing DesignWelded StructuresSheet Metal StructuresSpring DesignBolted JointsBearing Arrangement