Pitfall: A slender shaft with a length-to-diameter ratio >15 is turned without a follower rest
Consequence: Workpiece bending / vibration / out-of-tolerance dimensions
Correct: Add a follower rest + traverse against the tailstock offset + use a large feed
Pitfall: The depth of cut >0.5 times the cutter diameter
Consequence: Cutter vibration / chipping / breakage
Correct: Step down (each layer ≤0.3×D) / use a larger cutter diameter
Pitfall: Drilling deeper than 3 times the diameter without coolant or chip withdrawal
Consequence: The drill seizes or breaks
Correct: Withdraw every 3 diameters to clear chips + apply coolant
Pitfall: Grinding thin parts (thickness <5mm) without adequate coolant
Consequence: Thermal distortion / grinding burn / cracks
Correct: High-flow coolant / reduced feed / separate rough and finish grinding
Pitfall: The tap-drill depth in a blind hole < tap working length + 3 times the pitch
Consequence: The tap bottoms out → breakage
Correct: Hole depth = thread depth + 5× pitch (chip clearance)
Pitfall: Wire cutting starts at the edge of the workpiece (no start hole)
Consequence: Distortion / loss of accuracy
Correct: Drill a start hole (φ1~2mm) inside the workpiece
Turning a shaft with a length-to-diameter ratio >15 should use a steady rest or follower rest / without one → the workpiece bends, vibrates and tapers / the speed should be reduced by 30~50%
When facing, the tool must pass the center / cutting past the center leaves a raised boss, stopping short leaves a hollow / the tool tip should be aligned with the workpiece centerline
Threads with a large pitch (>4mm) should be cut in rough and finish passes / cutting them in one pass causes tool deflection → inaccurate pitch and heavy vibration / cut in several stepped passes
When milling thin-walled parts (wall thickness <5mm) use climb milling, a small depth of cut and multiple passes / use soft jaws when clamping / without these the tool deflects → dimensions out of tolerance
Wide flat surfaces (>100mm) should be machined with a face mill / an end mill that is too narrow gives low efficiency and visible steps / overlap each pass by ≥1/3
Thin parts (thickness <5mm) should be flipped and ground several times, with rough and finish grinding separated and adequate cooling / grinding straight to size in one pass → warping
When grinding hardened steel (HRC>50) select a soft wheel, use high coolant flow and reduce the depth of cut / a deep cut causes burn and micro-cracks
Punch a center mark before drilling, or drill a small pilot hole (φ2~3mm) first / without centering the drill slides → the hole position shifts
When the hole depth exceeds 3 times the diameter, retract the drill to clear chips and add coolant / without chip withdrawal the swarf clogs → the drill breaks
For tapping a blind hole the drill depth should be ≥ thread depth + 5× pitch / if it is < thread depth + 4× pitch the tap bottoms out → breakage
Too small a reaming allowance (the cutting action is lost) → the hole comes out undersized / too large (heavy load on the reamer) → poor surface finish / steel: 0.1~0.2mm / cast iron: 0.2~0.3mm
Wire cutting that starts at the edge distorts the workpiece and lowers accuracy / drill a φ1~2mm start hole / when accuracy is critical, start from the scrap side
EDM of a deep cavity (depth >3 times the diameter) flushes poorly → carbonized sludge accumulates / use reciprocating electrode lift, flushing or a larger pulse interval
Use a polarity with high electrode wear for roughing in EDM → high cost / rough with negative polarity (tool -) and finish with positive polarity (tool +)
When turning a grooved or relieved journal, the follower rest foot can drop into the groove and cause damage / fit a copper pad or use a follower rest with rollers
Use a face mill for large flat surfaces / its efficiency is 3~5 times that of an end mill / milling a large flat with an end mill → low efficiency and step marks
Cutting sheet metal (<3mm) with a grinding wheel → the cut edge overheats → heavy burrs and distortion / use a band saw, laser or plasma cutting
Tapping aluminum threads requires a cobalt high speed steel tap with a spiral flute / a general tap gives poor chip evacuation → tap breakage
A reaming allowance >0.3mm → heavy load on the reamer → poor surface finish and out-of-tolerance size / steel parts 0.1~0.2mm, cast iron 0.2~0.3mm
Broaching only machines through holes / a blind hole cannot be broached (the broach has no chip exit space) / use slotting for internal splines in blind holes
An excessive machining allowance wastes material and time / normally leave 2~3mm on the outer diameter, 2~4mm in the bore and 0.3~0.5mm for finish machining
Stress should be relieved after roughing (natural aging / annealing) before finish machining / if not separated → residual stress → distortion after finish machining
Grinding a slender shaft should use a shallow depth of cut (0.005~0.01mm) / a deep cut burns the workpiece and causes bending distortion / make several light passes
After grinding on an electromagnetic chuck the workpiece retains magnetism / demagnetize before removing it / otherwise the part is scrapped / use a demagnetizer
Stress concentrates at the thread run-out when turning a thread / provide a relief groove (width ≥3 times the pitch, depth ≥0.5mm) / without it → stress concentration → breakage at the thread root
The tailstock of a slender shaft should use an elastic (expanding) center / a fixed center over-constrains the workpiece → thermal expansion → bending
Pitfall: The design does not consider machining feasibility (for example the tool cannot clear, or the part cannot be clamped)
Consequence: The part cannot be machined / the design has to be changed
Correct: Consider the manufacturing process (DFM) at the same time as the design / refer to the machining process specification
When drilling thin-walled parts (<3mm) reduce the feed (0.02~0.05mm/r) / a normal feed distorts the workpiece and makes the hole out of round / place a wood block under the part
The wheel should be dressed regularly (with a diamond dresser) / an undressed wheel clogs → grinding temperature rises → the workpiece burns and the surface finish is poor
A deep hole drill with a length-to-diameter ratio >20 has poor rigidity and deflects / use a deep hole drill (gun drill / ejector drill) / split the operation into several passes
A reamer must never be reversed while withdrawing / reversing it dulls the cutting edges and shortens tool life / feed forward and withdraw forward
Drilling sheet metal (<2mm) should use a small diameter drill / a large diameter pushes the sheet before it is pierced, deforming it and making the hole out of round / support it with a wood block
When turning a slender shaft keep the depth of cut (ap) ≤2mm / too deep → vibration → poor surface finish and bending distortion
The counterbore allowance should be <3mm / too large → the counterbore drill vibrates → the hole is out of round and the finish is poor / expand in two passes
A boring bar with an overhang greater than 4 times the shank diameter has insufficient rigidity → vibration → poor hole accuracy / use a steady boring bushing
Grinding hardened steel (HRC>50) should use a CBN wheel or a soft wheel / an ordinary alumina wheel wears quickly → the size becomes unstable
The tap hole in aluminum should be 0.1~0.2mm larger than for steel (aluminum has a higher expansion coefficient) / too small → aluminum swarf sticks → tap breakage
Wire cutting sheet metal (<5mm) distorts the workpiece / rough cut first (leaving 0.5mm), let it stabilize, then finish cut / or cut from the scrap side
Stainless steel should be turned with a high-cobalt YG grade or coated carbide / ordinary YT grade causes chemical affinity → rapid tool wear
Coolant flow during grinding should be ≥40L/min (≥80L/min on a large grinder) / insufficient flow → high temperature in the grinding zone → burn
The blank diameter for thread rolling should equal the thread pitch diameter / too small → the thread crest is not filled / too large → the roller is overloaded and damaged
A positive rake angle (λ≥5°) should be used when facing thin-walled parts / without it the chips flow onto the machined surface → scratching
High-speed cutting (>200m/min) should use CBN or PCD inserts / ordinary carbide → short tool life → frequent tool changes
The thread relief groove should be at least 2.5 times the pitch wide and ≥0.5mm deep / too small → the tool collides when it withdraws → the tool is damaged
The wheel should be statically balanced before use / an unbalanced wheel → grinding vibration → chatter marks on the workpiece → loading on the wheel spindle
CNC programs should be verified against the first article, with the offsets set from the tool / a wrong offset → the first article is scrapped / measure the part after machining the first article
Use a soft wheel for soft materials and a hard wheel for hard materials / the wrong way round → low grinding efficiency and burn
When reaming, the reamer should be connected to the spindle with a floating coupling / a rigid connection → the reamer is not coaxial with the hole → the hole opens up
The finish machining datum should be the same as the roughing datum / if not, a positioning error results
Steel should be drilled with coolant (emulsion) / without it the drill wears quickly and seizes