Pitfall: welding thin plate with an electrode >φ3.2mm
Consequence: burn-through / severe distortion
Correct practice: use a φ2.5mm electrode / low current / fast welding on thin plate
Pitfall: no pickling and passivation treatment after welding stainless steel
Consequence: the weld blackens / corrosion resistance drops
Correct practice: pickling after welding (nitric acid + hydrofluoric acid) → passivation
Pitfall: welding cast iron (HT250) without preheating
Consequence: chilled (white cast iron) structure / cracks
Correct practice: preheat to 400~600℃ (overall or local) / slow cooling after welding