(1) Pitfall: welds concentrated on large structures
Correct practice: keep weld spacing ≥200 mm and avoid cross-shaped weld intersections
(2) Pitfall: no preheat before welding thick plate (>40 mm)
Correct practice: preheat to 100~150 ℃ for plate ≥40 mm, 150~200 ℃ for ≥60 mm
(3) Pitfall: no stress-relief annealing after welding
Correct practice: large welded structures must be stress-relieved at 580~620 ℃, soaking 1 h per 25 mm
(4) Pitfall: groove design too small
Correct practice: double-sided weld land ≤2 mm; single-sided root-pass land ≤1 mm
(1) Pitfall: impact loads not considered in mining machine structures
Correct practice: use a safety factor of 2~3 times the static load and fit buffers
(2) Pitfall: liner bolts spaced too far apart
Correct practice: liner bolt spacing ≤300 mm, always with lock nuts + spring washers
(3) Pitfall: poorly placed lubrication points
Correct practice: large bearing housings need a centralized lubrication system with accessible points
(4) Pitfall: no liner at discharge ports or chutes
Correct practice: line all material-contact faces of chutes with wear plate (10~20 mm thick)
(1) Pitfall: no belt-tracking devices at head or tail
Correct practice: fit self-aligning idlers (one set every 6~10 m)
(2) Pitfall: no anti-slip device on steep inclines
Correct practice: above 18° use a chevron belt or add cleats
(3) Pitfall: loading point off-center
Correct practice: loading chute centerline offset from the belt centerline ≤5 mm
(4) Pitfall: insufficient take-up travel
Correct practice: screw take-up travel ≥1%~1.5% of conveyor length
gravity take-up travel ≥2× the elastic elongation plus allowance
(1) Pitfall: wrong tooth hardness selection. Correct practice: pinion 30~50 HB harder than the wheel; for tooth surfaces ≤350 HB use quenched-and-tempered + induction hardening
(2) Pitfall: root fillet too small. Correct practice: R ≥0.38 m; a small fillet leads to fatigue fracture
(3) Pitfall: wrong lubrication. Correct practice: dip lubrication at v ≤12 m/s, spray above 12 m/s, extreme-pressure gear oil for heavy loads
(1) Pitfall: insufficient forging reduction. Correct practice: carbon steel ≥2.5, alloy steel ≥3.0, critical parts such as main shafts ≥4.0
(2) Pitfall: heating too fast causes internal cracking. Correct practice: ≤30 ℃/h below 300 ℃, ≤60 ℃/h from 300 to 800 ℃
(3) Pitfall: final forging temperature too low. Carbon steel 800~850 ℃, alloy steel 850~950 ℃
(1) Pitfall: cross joints not ground. Correct practice: weld-toe stress concentration factor is 2~3; must grind 0.5~1 mm
(2) Pitfall: welding residual stress ignored. Correct practice: residual stress can reach yield strength; post-weld heat treat at 600~650 ℃ or peen
(3) Pitfall: no transition at stiffener ends. Correct practice: provide a transition fillet R ≥50 mm at stiffener ends
(1) Pitfall: insufficient frame stiffness. Large jaw crusher frame wall ≥30 mm thick, rib spacing ≤500 mm
(2) Pitfall: liner bolts not locked. Use lock nuts + spring washers and check torque monthly
(3) Pitfall: poor bearing lubrication. Large crushers use forced-circulation lubrication; fill the grease cavity 1/3~1/2
Other quick references in this series:Welding PitfallsCasting PitfallsShaft System PitfallsSheet Metal PitfallsAssembly PitfallsHydraulic PitfallsPneumatic PitfallsShaft System DesignHousing DesignWelded StructuresSheet Metal StructuresSpring DesignBolted JointsBearing Arrangement