① Pitfall: Excessive step change in wall thickness
Correct practice: wall thickness ratio ≤2:1, with a gentle transition R≥0.5t in the transition zone
② Pitfall: Insufficient draft angle
Correct practice: ≥1° on outer surfaces, ≥1.5° on inner surfaces, ≥3° on textured surfaces
③ Pitfall: Rib root too thick
Correct practice: root thickness = 0.5~0.6t (too much thickness causes sink marks)
④ Pitfall: Sharp corner transitions
Correct practice: internal radius ≥0.5t, external radius ≥0.3t
⑤ Pitfall: Hole too close to the edge
Correct practice: hole-to-edge distance ≥ hole diameter (for holes <5mm) or ≥3mm
① Pitfall: Using fine threads directly. Correct practice: prefer coarse threads of M6 and above; use a metal insert below M4
② Pitfall: Insufficient draft angle. Outer threads ≥0.5°; inner threads need rotary or forced ejection
③ Pitfall: Threads too long. Length ≤1.5 times the diameter
Related quick references: Welding PitfallsCasting PitfallsShafting PitfallsSheet Metal PitfallsAssembly PitfallsHydraulic PitfallsPneumatic PitfallsShafting DesignHousing DesignWelded StructuresSheet Metal StructuresSpring DesignBolt ConnectionsBearing Arrangement