Design Pitfalls · Stamping Pitfalls (Quick Reference)

Stamped Part Structure Design Pitfalls

① Pitfall: Hole too close to the edge of a blanked part

Correct practice: hole-to-edge distance ≥1.5t, hole-to-hole distance ≥2t

② Pitfall: Flange height of a bend too small

Correct practice: straight flange height h≥3t+R

When h<R+2t the bend cannot be formed stably

③ Pitfall: Corner radius at the bottom of a deep drawn part too small

Correct practice: bottom radius R≥(3~5)t

Too small a radius causes cracking at the bottom

④ Pitfall: Too much scrap in the nesting layout

Correct practice: utilization ≥70% with row or diagonal nesting

Deep Drawn Part Design Pitfalls

① Pitfall: Flange width too large. Correct practice: b≤3t; a wider flange requires more drawing passes

② Pitfall: Punch corner radius too small. R_p≥(3~5)t, die radius R_d≥(4~8)t; too small a radius causes cracking at the bottom

③ Pitfall: Drawing clearance too small. Z=(1.0~1.1)t

Related quick references: Welding PitfallsCasting PitfallsShafting PitfallsSheet Metal PitfallsAssembly PitfallsHydraulic PitfallsPneumatic PitfallsShafting DesignHousing DesignWelded StructuresSheet Metal StructuresSpring DesignBolt ConnectionsBearing Arrangement

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL