Carbon content 0.17~0.23% / tensile strength σb≈410MPa
Applications: carburized parts (piston pins / small gears) / stamping parts
Heat treatment: carburizing 880~940℃ + quenching 780~800℃
Surface hardness HRC58~62 / core hardness HB140~180
Carbon content 0.32~0.39% / tensile strength σb≈530MPa
Applications: general shafts / connecting rods / bolts
Heat treatment: normalizing / quenched and tempered
Normalized hardness HB≤187 / quenched and tempered HB180~220
Carbon content 0.42~0.50% / tensile strength σb≥600MPa
Applications: transmission shafts / gear shafts / connecting rods / bolts / keys
Heat treatment: quenched and tempered, 820~840℃ quenching + 550~650℃ tempering
Quenched and tempered hardness HB220~250 / quenched hardness HRC48~55
Features: excellent overall mechanical properties / low cost / most widely used
Carbon content 0.47~0.55% / tensile strength σb≥630MPa
Applications: wear parts / gears / rolls
Heat treatment: quenched and tempered / quenched + medium-temperature tempering
Quenched and tempered hardness HB230~270 / quenched HRC50~58
Carbon content 0.57~0.65% / tensile strength σb≥680MPa
Applications: springs / elastic elements / rolls
Heat treatment: quenching + medium-temperature tempering
Hardness HRC45~55
Carbon content 0.62~0.70% / Mn 0.9~1.2% / tensile strength ≥980MPa
Applications: springs / spring leaves / spring washers / agricultural machinery
Heat treatment: quenching 790~830℃ + tempering 380~480℃
Hardness HRC45~55
Note: prone to quench cracking → oil quenching