Carbon content 0.18~0.24% / Cr 0.7~1.0%
Applications: carburized gears / small shafts / piston pins
Heat treatment: carburizing → quenching → low-temperature tempering
Surface HRC58~63 / core HRC35~45
Carbon content 0.37~0.44% / Cr 0.8~1.1% / tensile strength ≥980MPa
Applications: critical shafts / gears / connecting rods / bolts
Heat treatment: quenched and tempered, 840~860℃ oil quenching + 550~650℃ tempering
Quenched and tempered hardness HB240~285
Features: about 30% stronger than 45 steel / good hardenability
Carbon content 0.32~0.40% / Cr 0.8~1.1% / Mo 0.15~0.25%
Tensile strength ≥980MPa / σs≥835MPa
Applications: shafts / gears / bolts working at elevated temperature
Features: heat resistant / good tempering stability / for service below 500℃
Carbon content 0.38~0.45% / Cr 0.9~1.2% / Mo 0.15~0.3%
Tensile strength ≥1080MPa / σs≥930MPa
Applications: high-strength shafts / gears / crankshafts / forgings
Heat treatment: quenched and tempered, 840~860℃ + tempering
Quenched and tempered hardness HB280~340
Carbon content 0.36~0.44% / Cr 0.6~0.9% / Ni 1.25~1.75% / Mo 0.15~0.25%
Tensile strength ≥980MPa
Applications: shafts and aircraft parts requiring high strength and toughness
Features: outstanding overall properties / high cost
Carbon content 0.35~0.42% / Cr 1.35~1.65% / Mo 0.15~0.25% / Al 0.7~1.1%
Applications: precision spindles / boring bars / ball screws
Heat treatment: quenched and tempered + nitriding
Surface hardness after nitriding HV900~1100
Related quick references: Heat Treatment Process ParametersCarbon Structural SteelQuality Carbon SteelBearing SteelTool SteelStainless SteelCast IronAluminium AlloySteelsNon-ferrous AlloysHeat Treatment ProcessesCommon SteelsCast Iron & Non-ferrous Metals