Carbon content 0.75~0.84% / quenched HRC62~64
Applications: punches / chisels / woodworking tools
Heat treatment: quenching 760~780℃ water cooling + tempering 160~200℃
Carbon content 0.95~1.04% / quenched HRC62~64
Applications: files / taps / dies / stamping dies
Heat treatment: quenching 760~780℃ water cooling + tempering 160~200℃
Carbon content 0.70~0.80% / W 17.5~19% / Cr 3.8~4.4% / V 1.0~1.4%
Red hardness: retains above HRC60 at 600℃
Applications: high-speed lathe tools / milling cutters / drills / hobs
Heat treatment: quenching 1260~1290℃ + tempering 560℃ × 3 times
Hardness HRC63~66
Carbon content 1.45~1.70% / Cr 11~12.5% / Mo 0.4~0.6% / V 0.15~0.3%
Applications: cold stamping dies / cold extrusion dies / thread rolling dies
Heat treatment: quenching 950~1000℃ + tempering
Hardness HRC58~62
Related quick references: Heat Treatment Process ParametersCarbon Structural SteelQuality Carbon SteelAlloy Structural SteelBearing SteelStainless SteelCast IronAluminium AlloySteelsNon-ferrous AlloysHeat Treatment ProcessesCommon SteelsCast Iron & Non-ferrous Metals