Carbon content 0.95~1.05% / Cr 1.30~1.65%
Hardness after quenching HRC60~66
Applications: bearing rings / rollers / balls / precision measuring instruments
Heat treatment: spheroidizing anneal → quenching 830~860℃ → tempering 150~170℃
Related quick references: Heat Treatment Process ParametersCarbon Structural SteelQuality Carbon SteelAlloy Structural SteelTool SteelStainless SteelCast IronAluminium AlloySteelsNon-ferrous AlloysHeat Treatment ProcessesCommon SteelsCast Iron & Non-ferrous Metals