Carbon content ≤0.08% / Cr 18~20% / Ni 8~10.5%
Tensile strength ≥520MPa / yield strength ≥205MPa
Applications: food machinery / chemical equipment / decoration
Features: good corrosion resistance / cannot be strengthened by heat treatment / work hardening
Maximum service temperature 800℃
Carbon content ≤0.08% / Cr 16~18% / Ni 10~14% / Mo 2~3%
Tensile strength ≥520MPa
Applications: marine environments / chemical / medical
Features: more resistant to Cl- corrosion than 304 / acid resistant
The Mo content improves pitting resistance
Carbon content ≤0.12% / Cr 16~18%
Tensile strength ≥450MPa
Applications: home appliances / kitchen equipment / decoration
Features: low price / magnetic / corrosion resistance inferior to 304
C:0.08~0.15% / Cr:12~14% / σb:540 / σs:345
Can be strengthened by heat treatment / quenched HRC40~45 / applications: cutting tools / valve discs
C:0.16~0.25% / Cr:12~14% / σb:600 / σs:390
Quenched HRC45~51 / applications: knives / nozzles / bearings
C≤0.03% / Cr:18~20% / Ni:8~12% / σb:480 / σs:177
Resistant to intergranular corrosion / welded parts / chemical equipment
C≤0.03% / Cr:16~18% / Ni:12~15% / Mo:2~3% / σb:480 / σs:177
Marine environments / medical / chemical / better Cl- resistance than 304
Related quick references: Heat Treatment Process ParametersCarbon Structural SteelQuality Carbon SteelAlloy Structural SteelBearing SteelTool SteelCast IronAluminium AlloySteelsNon-ferrous AlloysHeat Treatment ProcessesCommon SteelsCast Iron & Non-ferrous Metals