Product Design · Injection Molding Process (Quick Reference)

Injection Molding Machine Clamping Force Calculation

【Clamping Force Calculation】

F_s=K×P_c×A

F_s required clamping force (kN), K safety factor (1.1~1.2)

P_c melt pressure in the cavity (MPa), typically 30~50MPa

A projected area of the part (mm²)

【Calculation Case】

Projected area of the part 50000mm², cavity pressure 40MPa

F_s=1.2×40×50000/1000=2400kN

→ select an injection molding machine with a clamping force ≥3000kN

Injection Molding Process Parameter Setting

【Barrel Temperature Setting】

Nozzle temperature: 5~10℃ lower than the front barrel zone (prevents drool)

Three barrel zones: rear zone 10~20℃ below the melting point, middle zone 10~20℃ above, front zone 20~30℃ above

【Injection Pressure】

Typically 80~140MPa

Wall thickness 0.5~2mm: high pressure 110~140MPa

Wall thickness 2~5mm: medium pressure 80~110MPa

Wall thickness >5mm: low pressure 60~80MPa

【Cooling Time】

t=δ²×cp×ρ/(2×λ×π²)×ln(8/π²×(Tm-Tw)/(Te-Tw))

Injection Molded Part Defect Analysis and Countermeasures

【Sink / Void】

Causes: insufficient holding pressure / short holding time / gate freezes too early

Countermeasures: ① increase the holding pressure by 10%~20% ② extend the holding time ③ enlarge the gate

【Flash】

Causes: insufficient clamping force / mould deformation / debris on the parting line

Countermeasures: ① raise the clamping force ② check the parting line parallelism ③ clean the parting line

【Weld Line】

Causes: temperature drop where the melt fronts meet / poor venting

Countermeasures: ① raise the melt and mould temperatures ② add vent grooves ③ increase the injection speed

【Air Trap】

Causes: gas in the cavity cannot escape

Countermeasures: add vent grooves (depth 0.02~0.05mm) and reduce the injection speed

Mould Shrinkage Rate and Part Dimensional Tolerance

【Common Plastic Shrinkage Rates】

ABS: 0.4%~0.7%

PP: 1.0%~2.5% (strongly affected by crystallinity)

PC: 0.5%~0.7%

PA66: 1.0%~2.0% (affected by moisture absorption)

POM: 1.8%~2.5%

PET: 1.2%~2.0%

PBT: 1.5%~2.5%

【Mould Cavity Dimension Calculation】

D_m=D_p×(1+S)+Δ/2

D_m cavity dimension, D_p nominal part dimension, S shrinkage rate, Δ tolerance

Injection Molding CAE Analysis Applications

【Purpose of CAE Analysis】

Predict filling / packing / cooling / warpage during injection molding, optimize the mould design and reduce the number of trial shots.

【Analysis Workflow】

① Mesh generation → ② Material selection and process parameter setting → ③ Filling analysis → ④ Packing analysis → ⑤ Cooling analysis → ⑥ Warpage analysis

【Key Outputs】

Filling end temperature (≥ melting temperature + 20℃)

Peak injection pressure (≤ 90% of the machine rated pressure)

Weld line position and angle (a merge angle ≥135° gives good strength)

Warpage deformation (should be smaller than the part tolerance)

【Common Issues】

Unbalanced filling: the gate position or runner size needs to be optimized

Injection Mould Cooling System Design

【Water Channel Design】Diameter 6~16mm, spacing 2.5~5 times the channel diameter, distance to the cavity 1.5~2 times the channel diameter

【Cooling Time】t_c=δ²/(π²×α)×ln(8/π²×(Tm-Tw)/(Te-Tw))

【Issues】An excessive channel spacing causes uneven cooling and warpage; an inconsistent channel-to-cavity distance causes a non-uniform mould temperature distribution

Gate Type Selection Guide

【Types】① Edge gate is the most common for multi-cavity moulds ② Sprue gate on a three-plate mould gives automatic cutting ③ Submarine gate feeds from under the parting line ④ Fan gate for large thin-walled parts ⑤ Ring gate for cylindrical parts to avoid weld lines

【Dimensions】Width 0.5~0.8× the wall thickness, thickness 0.3~0.6× the wall thickness, length 0.5~1.5mm

【Hot Runner】No runner scrap shortens the cycle, but the cost is high and colour changes are difficult; suited to high volume parts with high appearance requirements

Injection Mould Ejection System Design

【Methods】Ejector pin ejection is the most common (diameter ≥2.5mm), stripper plate ejection suits thin-walled large area parts, ejector sleeve suits cylindrical parts, pneumatic ejection suits deep cavity parts

【Parameters】Ejection stroke ≥ part height + 5~10mm, load per ejector pin ≤200N/mm²

【Reset】Reset pins / springs / hydraulics

Plastic Material Selection Guide

【Engineering Plastics】ABS has balanced general properties for housings / appliances, PC has high strength with transparency and impact resistance for lenses / guards, PA66 is wear and oil resistant for gears / bearings, POM has high stiffness for gears / cams, PP is light and chemical resistant for chemical containers

【Selection】Service temperature PP≤100℃ ABS≤80℃ PC≤120℃ PA≤150℃; wear resistance POM≥PA66>PC>ABS>PP; cost PP≤ABS<PA66<PC<POM

Related quick references: Stamping ProcessDie Casting ProcessSurface TreatmentMold StructureRunner SystemCooling SystemMold MaterialsPlastic MaterialsInjection Molding DefectsMold MachiningHot Runner SystemAutomotive MoldsForging Dies

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL