Pulse discharge between the tool electrode and the workpiece generates a very high temperature (above 10000℃) that erodes the material
Roughing: current 6~12A, pulse width 200~600μs, Ra=6~12μm
Semi-finishing: current 3~6A, pulse width 100~200μs, Ra=3~6μm
Finishing: current 1~3A, pulse width 10~50μs, Ra=1~3μm
Graphite: fast machining speed (2~3 times copper), high electrode wear, suited to roughing
Pure copper: stable machining, low electrode wear, suited to precision machining
Copper tungsten: the lowest electrode wear, suited to deep narrow slots
Roughing: 0.3~0.5mm per side
Finishing: 0.05~0.15mm per side
Kerosene or a dedicated EDM oil
Filtration accuracy ≤5μm
Electrode wire: molybdenum wire (φ0.12~0.20mm)
Wire feed speed: 6~12m/s
Machining accuracy: ±0.01~0.02mm
Surface roughness: Ra=1.6~3.2μm
One cut is sufficient
Electrode wire: brass wire (φ0.1~0.3mm)
Wire feed speed: 0.01~0.1m/s (single use)
Machining accuracy: ±0.002~0.005mm
Surface roughness: Ra=0.2~0.8μm
Multiple cuts are needed (rough cut + 3~5 finishing passes)
Fast wire: 30~80mm²/min
Slow wire: 5~30mm²/min (the higher the accuracy, the slower the speed)
Fast wire: general mould punches / dies
Slow wire: precision mould inserts / precision blanking dies
Roughing: corner radius cutter (Φ12~25R0.5~1) or a square shoulder mill
Finishing: ball nose cutter (Φ3~12) or a corner radius cutter (Φ6~12R1~3)
Machining hardened steel (HRC>45) requires CBN or coated carbide tools
Rough milling: 2500~5000rpm, depth of cut 0.5~2mm, feed 800~2500mm/min
Finish milling: 5000~12000rpm, depth of cut 0.1~0.3mm, feed 1000~3000mm/min
Ball nose cutter stepover: 0.1~0.3mm (rough), 0.03~0.1mm (finish)
Surface roughness control: the smaller the stepover the smoother the surface
④ Corner clearing: a small tool cleans the residual areas
⑤ Polishing: manual polishing after EDM (400#~1200# sandpaper)
Related quick references: Injection Molding ProcessStamping ProcessDie Casting ProcessSurface TreatmentMold StructureRunner SystemCooling SystemMold MaterialsPlastic MaterialsInjection Molding DefectsHot Runner SystemAutomotive MoldsForging Dies