Small end diameter d=nozzle diameter + 0.5~1.0mm (typically φ3~φ6mm)
Taper: 1°~2° (facilitates ejection)
Large end diameter D=d+2×L×tan(α)
L sprue runner length (typically 40~80mm)
Material: SKD61 quenched to HRC38~42
The locating bore mates with the machine nozzle locating ring φ100/φ120
Spherical radius R=nozzle radius + 0.5~1mm
A cold slug well is provided at the end of the sprue runner, depth 5~10mm
Z-puller: forces ejection
Inverted taper: automatic ejection
The sprue runner should be as short as possible (reduces pressure loss and material waste)
Round: minimum pressure loss but high machining cost (requires a ball mill)
Trapezoidal: the most common and easy to machine, recommended dimensions: base width W=6~12mm, height h=2/3W
U-shaped: between round and trapezoidal
Diameter d=part wall thickness×1.2~1.5 + 1.5mm
Common range: φ4~φ12mm
Natural balance: the distance from each cavity to the sprue runner is equal
Artificial balance: adjust each runner cross-section so that filling is synchronised
Recommended: prefer natural balance on multi-cavity moulds
The longer the runner, the greater the pressure loss
Each 100mm of runner costs about 10%~20% pressure loss
The runner is moulded together with the part and separated after ejection
Advantages: simple structure and low cost, easy colour change, easy maintenance
Disadvantages: produces runner scrap (10%~50% of the part weight) and requires extra granulation and recycling equipment
Application: small batches / frequent multi-colour and multi-material changes
The runner stays molten at all times, so no scrap is produced
Advantages: no scrap, saves material (10%~30%), shortens the cycle, good gate quality
Disadvantages: high cost (10,000~50,000 CNY per system), difficult colour changes (the runner must be cleaned), strict temperature control
Application: high volume / precision parts / expensive plastics
Under 50,000 parts per year: cold runner
50,000~500,000 parts per year: depends on the material price (a hot runner pays off for engineering plastics)
Over 500,000 parts per year: hot runner
① Parting line vent groove: the most common
② Ejector pin clearance venting: gap between the pin and its hole 0.01~0.02mm
③ Insert clearance venting: fit clearance of the inserts 0.01~0.02mm
④ Porous steel insert: local venting (sintered porous material)
⑤ Vacuum venting: used for precision / high-gloss moulds
Depth: amorphous plastics (ABS/PC) 0.015~0.03mm
Crystalline plastics (PA/POM/PP) 0.03~0.05mm
Width: 3~25mm
Length: 10~30mm (it can then be deepened to 0.1~0.3mm to let the air escape)
At the end of filling (where the melt arrives last)
At weld lines
At the bottom of deep cavities
At dead corners / insert boundaries
Trapped air causes burn marks / short shots / low weld line strength
Related quick references: Injection Molding ProcessStamping ProcessDie Casting ProcessSurface TreatmentMold StructureCooling SystemMold MaterialsPlastic MaterialsInjection Molding DefectsMold MachiningHot Runner SystemAutomotive MoldsForging Dies