Drying Conditions for Common Injection Moulding Plastics

【Hygroscopic Plastics (must be dried before injection)】

ABS: 80~90℃×2~4h, moisture <0.05%

PC: 120℃×4~6h, moisture <0.02%

PA6/66: 80~90℃×6~12h, moisture <0.1%

PMMA: 80~90℃×4~6h, moisture <0.04%

PET: 130~160℃×4~6h, moisture <0.02%

【Non-hygroscopic Plastics (generally no drying required)】

PP/PE/PS/POM — usually no drying needed

POM with a small amount of moisture can be dried at 80℃×1~2h

【Drying Cautions】

① The drying temperature must not be too high (PC above 130℃ degrades)

② Use the material immediately after drying (PA reabsorbs moisture within 15min in air)

③ The hopper holding temperature should match the drying temperature

④ The residence time of the plastic in the hopper should not exceed 2h (long heating causes degradation)

Comparison of Flow and Moulding Performance of Engineering Plastics

【Flowability (MFR melt flow rate)】

PP: MFR=2~30g/10min (good flowability)

ABS: MFR=2~30g/10min (medium flowability)

PC: MFR=3~30g/10min (poor flowability)

PA6: MFR=8~40g/10min (good flowability)

POM: MFR=3~30g/10min (medium flowability)

【Shrinkage Rate】

PP: 1.0%~2.5% (crystalline, large shrinkage)

ABS: 0.4%~0.7% (amorphous, small shrinkage)

PC: 0.5%~0.7% (amorphous, small shrinkage)

PA66: 1.0%~2.0% (crystalline, affected by moisture absorption)

POM: 1.8%~2.5% (crystalline, large shrinkage)

PBT: 1.5%~2.5% (crystalline)

【Reinforcement Characteristics】

Plastics with good flowability (PP/PA6) suit thin walls and long flow paths

Plastics with poor flowability (PC/PC+ABS) need a large gate and a high temperature

【Effect of Glass Fibre Reinforcement】

After glass fibre reinforcement: the shrinkage rate drops by 50%~70%, the flowability decreases and the mould wear increases

Plastic Additives and Modified Material Selection

【Glass Fibre Reinforcement (GF)】

GF10~GF50: glass fibre content 10%~50%

Tensile strength improves by 2~4 times, the heat distortion temperature rises by 30~80℃

But brittleness increases and the shrinkage rate drops by 50%~70%

The mould must use hardened steel (SKD61) to prevent wear

【Flame Retardant Grades (V0/V1/V2)】

UL94 V0: self-extinguishing 10 seconds after the flame is removed, no dripping

Common: PC/ABS V0, PA66 V0

Note: the flame retardant reduces the mechanical properties and the weather resistance

【Toughened Grades】

Adding an elastomer raises the impact strength

Typical: toughened PA6 (impact strength improves by 3~5 times)

But the stiffness and the hardness drop

【UV Stabilised Grades】

Adding UV absorbers and carbon black

Application: outdoor products / automotive exterior trim

Colour options are limited (usually black)

Related quick references: Injection Molding ProcessStamping ProcessDie Casting ProcessSurface TreatmentMold StructureRunner SystemCooling SystemMold MaterialsInjection Molding DefectsMold MachiningHot Runner SystemAutomotive MoldsForging Dies

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL