(1) Shielding gas flow too low or too high
(2) Wire or base metal has oil / rust
(3) Excessive air flow (wind speed > 2 m/s)
(4) Welding gun nozzle clog
(5) Insufficient gas purity
(1) Adjust shielding gas flow
(2) Clean welding area
(3) Provide wind protection
(4) Clean nozzle
(5) Replace with high-purity gas
(1) Shrinkage deformation
(2) Angular deformation
(3) Bending deformation
(4) Twisting deformation
(1) Reverse deformation — preset opposite-direction deformation
(2) Rigid fixing — use fixtures to restrain deformation
(3) Reasonable welding sequence — symmetrical / skip welding
(4) Preheating — reduce temperature gradient
(5) Post-weld correction — flame / mechanical straightening