Parts produced by the same mold have inconsistent dimensions, exceeding tolerance.
(1) Barrel temperature fluctuation (loose heater contact or thermostat failure)
(2) Unstable holding pressure (hydraulic oil temperature variation)
(3) Uneven mold temperature (cooling channel blockage)
(4) Raw-material batch variation (different MFR melt index)
(1) Take 20 consecutive parts and measure key dimensions for CPK analysis
(2) Check actual vs set temperature at each zone
(3) Check cooling water temp difference (inlet/outlet ≤ 5°C)
(1) Calibrate thermostat, check heaters
(2) Stabilize hydraulic oil temperature (add cooler, keep 40~50°C)
(3) Clean cooling channels
(4) Use same batch material for same product
Silvery streaks or foggy marks along flow direction on part surface.
(1) Insufficient raw-material drying (ABS moisture should be < 0.05%, PC < 0.02%)
(2) Excessive barrel temperature causing material decomposition
(3) Melt residence time in barrel too long
(4) Poor venting, residual gas in cavity
(1) Dry raw material: ABS 80~90°C × 2~4 h, PC 120°C × 4 h
(2) Lower barrel temperature, especially nozzle temperature
(3) Shorten molding cycle (reduce residence time)
(4) Add vent slots to mold (depth 0.02~0.03 mm)
(5) Increase injection speed to give gas enough time to escape